Classification | Rubber And Plastic raw materials |
Elongation at break | 800% |
Money Scorch | 25 |
Ash content | 1.5% |
Volatile matter | 1.5% |
Appearance | Beige ( or light brown) chips |
Shelf life | 12 months |
Application
For making rubber products such as hoses, cable sheath.
Description
A sulfur and xanthogen mixed-modified polychloroprene rubber with medium crystallization rate, the density is 1.23. It has good resistance totear and flexure, superior processibility over sulfur-modified types and superiorresistant properties to ozone, sunlight, weather, oil, grease and flame. It issimilar to Du Pont’s neoprene GW.